Hi Genny,
To further the info from Phil, here's some info regarding the copper
screening material: http://www.twpinc.com/rfi.html
You can make a screen cage with 2x4's, mesh, lag bolts and washers. The
critical thing would be to ensure that the washer completely covers the hole
made in the screen for the lag bolt to pass through. One side note, the
cage doesn't need to be grounded, it should be isolated.
There are some commercially available products that may fit your needs, such
as a portable "tent" that is made of aluminum poles and EMI shielded
material. If I can find that information, I'll pass it along later....
Good Luck.
Steve Sauer
Mfg Engineer
Xetron Corporation
-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
You could try copper window screen material....
I seen this successfully used for a high voltage faraday cage and it is also
used on our EMC compliance test room.
Phil Nutting
-----Original Message-----
From: Genny Gibbard [mailto:[log in to unmask]]
Looking for ideas - preferably more along the lines of homemade basket
idea..... RF screen or something that we can mount and ground between the
benches to reduce what we call 'crosstalk'.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|