Subject: | |
From: | |
Date: | Mon, 17 Jul 1995 07:48:40 -0400 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
In addition, the IPC Electrochemical Migration Task Group has compiled a
bibiliography with abstracts and reviews regarding all present day
electromigration articles. It should be available as IPC-TR-476A.
Doug Pauls
|
|
|