TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sat, 17 Mar 2001 10:44:06 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (60 lines)
Steve

Most water-soluble liquid fluxes do contain a dye. The most violent was
the old Lonco 3355 stuff which was a bright magenta (I think the
colorant may have been basic fuschin). The Alpha equivalent was a light
blue and I've also seen green (Kester?). We, in a previous life, asked a
couple of manufacturers, ten years ago, whether a heat-resistant dye
could be added to w/s cored wire to make it evident when retouches
hadn't been cleaned, but they both prevaricated.

The coloured labels idea is the best, provided you have one on each
assembly, as well. This can be applied to liquid, wire and paste. The
operator then knows that he has to match the assembly label to the flux
label. Alternatively, if you have control of the bare PCB fab, you can
make the legend in light pink, blue and green to match with the labels.

Brian

"Stephen R. Gregory" wrote:
>
> Hi ya'll!
>
> We use three different flux types in our processes here. No-clean (for hand
> soldering items that can't be cleaned...unsealed switches, etc.) RMA (because
> some of our customers require it), and OA (for everything else...).
>
> We seem to occasionally have a problem with our operators picking up the
> wrong bottle of flux thinking it is no-clean, but it is OA...and yes, the
> bottles are labeled, but it still happens...
>
> Is there some sort of dye that could be put into the flux that wouldn't hurt
> the chemistry of the flux, would wash off completely, and not turn other
> things colored? I'm thinking that if there's a really different color to OA
> flux, it would lessen the chance picking-up the wrong bottle, and you can
> easily tell when OA's haven't been cleaned from the board.
>
> Just trying to make things "monkey-proof" if ya' know what I mean...hehehe.
>
> -Steve Gregory-
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2