TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Wed, 20 Sep 2006 10:57:29 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Smith <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Steve Smith <[log in to unmask]>
Parts/Attachments:
text/plain (57 lines)
I have some in DWG/DXF & Altium formats.

My regards,
Steve Smith, C.I.D.
Product Engineer

Staco Energy Products Co.
301 Gaddis Boulevard.
Dayton, OH 45403
Telephone: (937) 253-1191 Ext. 158
Fax: (937) 253-1723
E-mail: [log in to unmask]  
Web Site: www.stacoenergy.com 
& www.stacopower.com 

DISCLAIMER AND/OR CONFIDENTIALITY NOTICE:   
This message, including any attached materials, is intended solely for the use of the individual or entity to whom it is addressed and may contain information that is privileged, confidential, and exempt from disclosure under applicable law.  If the reader of this electronic mail transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this communication is strictly prohibited.  If you have received this communication in error, please e-mail or call Staco Energy Products Co. at (937) 253-1191.  Thank you for your cooperation.
 


> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve Gregory
> Sent: Wednesday, September 20, 2006 9:02 AM
> To: [log in to unmask]
> Subject: [TN] Small Triangular ESD labels...
> 
> 
> Morning All!
>  
> I'm looking for a source for some small triangular ESD symbol labels,
> the one that has the little hand with a line through it, 
> about 5mm on a
> side. They need to go on a face plate frame for an assembly. 
> I've looked
> at many web pages, but all I can find is the type of ESD 
> labels that you
> would put on static bags which won't work...
>  
> I was hoping I could find something off-the-shelf, but it looks like I
> might have to order something custom unless somebody knows a 
> source for
> something like that.
>  
> Thanks!
>  
> -Steve Gregory-  

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2