Sorry for the delay but here are the plastic ball solder joint images in a
zip file.
Looking at the images I obviously have never finished grinding and polishing
the sections so that is why they are not perfect, work in progress. I
obviously had to stop working on this little project and move on to
something else between 204 and 07?
www.ASKbobwillis.com/bobwillisballs.zip
David Bernard of Dage has some more of the plastic ball x-ray images and has
also produced some CT images.
Hope they help.
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
Book your place on Bob's "Step by Step Failure Analysis Workshop" 14th May
www.ASKbobwillis.com/faworkshops.pdf
New "Printed Board Inspection & Quality Control" 3 July
www.ASKbobwillis.com/PCBworkshop.pdf
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|