Hi Pete,
Thanks for your response. My post was somewhat confusing, as by OSP over
Immersion Silver I actually meant to use Semblant SPF or SCI for corrosion
protection. I was advised by a member to re-post it with correction.
I really wanted to know if Immersion Silver can be selectively applied to
certain part of circuit, which I know now is not correct. Rest of the
board will still have solder mask, so SPF or SCI can be applied only to
the part of the circuit with no solder mask.
I have been adjusting trace impedance to take in to account the solder
mask effect. However it still produces non-uniform impedance due to
uneven application of solder mask.
Regards
Ravinder Ajmani
HGST, a Western Digital company
[log in to unmask]
5601 Great Oaks Pkwy.
San Jose, CA 95119-1003
www.hgst.com
Pete <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/07/2012 06:21 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Pete <[log in to unmask]>
To
<[log in to unmask]>
cc
Subject
Re: [TN] PCB Fab process
Ravinder,
If you are using both Immersion silver and OSP, I believe that the
Immersion Silver will be the replacement for the HASL, OSP can be applied
selectively (not the entire board). But neither provide good long term
corrosion protection over traces. If you must route high speed traces on
outer layers, consider adjusting the trace width of the high speed traces
to account for a solder mask cover.
You may want to subscribe to the Designer's council listserver for more
advice on PCB design questions.
Pete
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|