TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jeffrey Bush <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Date:
Tue, 21 Mar 2006 08:03:00 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (76 lines)
I would recommend using DSTF foils and not scrubbing, but rather using a
chem clean system to remove the chromate conversion and any other
contaminates present.  Scrubbing introduces problems in thinner
dielectrics and you resulting post lamination true position will be
unique panel to panel.

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED 
           76 Technology Drive - POB 1890 
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 21
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/> 
                           

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of McKinley Ken Civ 402
EMXG/MAILM
Sent: Tuesday, March 21, 2006 6:36 AM
To: [log in to unmask]
Subject: [TN] Cleaning PWB's before imaging
Sensitivity: Private

Trying to find out the proper way to clean printed wiring boards prior
to
imaging.

Should the board go through sulfuric bath rinse with DI water before
scrubbing?

Also the fact should I be using DI water at all in this stage of the
process?



Ken McKinley  402d EMXG/MXVD

740 Page Rd.

Robins Air Force Base Ga.  31098

ph: 478-926-2225 Fax: 478-926-7164

[log in to unmask] <mailto:[log in to unmask]>




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2