I was told by the manufacturer of paralyne that you will need a temp of 900
degrees f to remove paralyne. Not a good option. Plasma or bead blast will
do the job.
-----Original Message-----
From: WEEKES, MICHAEL HS-SNS [mailto:[log in to unmask]]
Sent: Thursday, December 05, 2002 10:58 AM
To: [log in to unmask]
Subject: [TN] reworking paralyne (paraxylene) coated BGAs and uBGAs
Hello fellow Technetters:
Anyone have any experience removing paralyne (paraxylene) coated BGAs and
uBGAs with conventional air vac DRS 24 type hot air equipment - I tried
conventional reflow profiles and it was very unsuccessful.
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|