It leads to separation anxiety.
It depends.
There are specific design and end use environment requirements, which
could have a potential impact on whether the capacity existed to allow
some delamination. A few rules of thumb( if this was for lead-free, it
would be green thumb):
* Do not accept if it decreases dielectric spacing by more than
50%
* Do not accept if it propagates
* Do not accept for high voltage applications
* Do not accept if humidity is a concern
* Do not accept if minimum dielectric spacing is 0.006 inches or
less
* Do not accept if it fails CAF testing
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pasquito, Helena
Sent: Tuesday, September 12, 2006 9:45 AM
To: [log in to unmask]
Subject: [TN] Delamination
Hi TechNetters,
Let me ask a question; I know delamination is bad, but why? What is the
failure mode to the board when a board delaminates and would there ever
be an instance that a board that delaminates is still OK to use? This
is a Class 3 application. Yes, I know what the IPC standards say but
not real sure about the board process. Yes, I "googled" and there is a
lot of stuff out there. Maybe someone can recommend some reading
material (hopefully short and sweet and to the point).
Thanks!
Helena
Helena Pasquito
Manufacturing Skills Instructor
M/A-COM, Tyco Electronics
1011 Pawtucket Blvd., M/S 107
Lowell, MA 01853
978-442-5024
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|