text/plain (32 lines)
     Hello TechNet Again!
     I have another question.  Is there data concerning soldering iron
     temperatures as related to no-clean/low-residue flux?

     The data I hope to see is on solder iron temperature(s) that is
     preferrable when handsoldering using a no-clean/low-residue flux.

     BACKGROUND:  I have seen differences in flux residues and their affect
     at incircuit test.  I am looking for a relationship of soldering iron
     temperature vs. dwell time vs. flux type.  The flux characteristics
     change.  I have had very good results with the flux in a solder paste
     to the point there is no affect at Incircuit test.  Using that same
     flux type for handsoldering I have seen a residue that is close but is
     more stringy than the residue from the paste.  I am wondering about
     the irom temperature.  Could it be to hot? Is it starting to
     polymerize because of the heat?

     Thanks
     Ron H.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2