If you want to evaluate lead free HASL I suggest you specify SnCu+ni or SAC.
If flatness is critical specify Horizontal leveling. If you looking to add a
thickness spec. Ask for double the minimum and half the maximum you would
normally spec for SnPb HASL.
 We would be happy to process small quantities FOC for you.

-----Original Message-----
From: Kane, Joseph E [mailto:[log in to unmask]]
Sent: Thursday, July 01, 2004 10:04 PM
To: [log in to unmask]
Subject: [TN] Specifying PWB Finishes


We're preparing to order some test boards with alternative finishes for
lead-free testing, including immersion tin and OSP over bare copper.  Can
anyone suggest how we might specify these board finishes in a drawing note?
Our existing drawings pretty much specify only the material and the
thickness, something like "immersion gold, xxx thick, over electroless
nickel, xxx thick."

Joe Kane
BAE SYSTEMS Controls
Johnson City, NY

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2