Jim, Remember the Solder Pots we used for Tinning Wires? It works great for
stripping the insulation of the Magnet Wire.

-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: Wednesday, October 31, 2001 1:11 PM
To: [log in to unmask]
Subject: Re: [TN] STRIPPING MAGNET WIRE


Can't find ant info on Beck chemicals (EPOXYSTRIP T-251-C) or Insulstrip
Jell.  Do you have any additional information?

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879



        -----Original Message-----
        From:   Matt Stanik [SMTP:[log in to unmask]]
        Sent:   Wednesday, October 31, 2001 12:46 PM
        To:     [log in to unmask]
        Subject:        Re: [TN] STRIPPING MAGNET WIRE

        Beck Chemicals of Cleveland, Ohio used to sell a product called
        EPOXYSTRIP T-251-C specifically for removing insulating varnishes
        and epoxies from wire and such. It worked great.


        > Looking for a recommendation for a chemical stripper to strip
bi-filar (?)
        > magnet wire.  Any suggestions?
        >


----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2