TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Afri Singh <[log in to unmask]>
Date:
Thu, 22 Jan 1998 23:39:47 -0500
Content-Type:
TEXT/PLAIN; charset=US-ASCII
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Afri Singh <[log in to unmask]>
Parts/Attachments:
TEXT/PLAIN (28 lines)
Can anyone shed some light on a problem i am having in my lam dept.
We are getting pockets of air (bubbles) trapped in low pressure areas
towards the middle of the panel
Seen only on the top or bottom panel of each book
This only happens on cores with 2-3 oz cu.

So far we have tried
heat rise 12 -16 F /min
b-stage with more resin- we are using 7628 only
vacume assist press and hydrolic
low pressure vs high
no kiss cycle
flatness of plates
not able to modify the pettern

  thank you for any suggestions

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################

ATOM RSS1 RSS2