TECHNET Archives

September 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 27 Sep 2012 14:13:38 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Karen Tellefsen <[log in to unmask]>
Message-ID:
<OFABCD0984.B91A5C3A-ON85257A86.0063F653-85257A86.00641EDF@LocalDomain>
Subject:
From:
Karen Tellefsen <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (80 lines)
I'd be more concerned about SIR than lack of reflow.  The concept of 
activation is misleading. 

Karen Tellefsen - Electrical Testing
Alpha / 109 Corporate Blvd./ S. Plainfield, NJ 07080
[log in to unmask]
908-791-3069




From:   Robert Kondner <[log in to unmask]>
To:     <[log in to unmask]>, 
Date:   09/27/2012 01:13 PM
Subject:        [TN] Flux Activation Temps
Sent by:        TechNet <[log in to unmask]>



Hi,

 

I was looking though some paste datasheets which show a paste "Family"
available in different alloys. 

 

My Question:

 

Is a single flux formulation being used with these different alloys? It
seems so.

 

But the various melting point have a serious range. And I remember from my
college chemistry days that reaction rates double for every 10 C rise in
temp. (Is that still correct?) So I would expect fluxes to be relatively
"Inactive" al low leaded temps but then going super-fast at higher lead 
free
temps.

 

Can anyone clarify? Is it a real issue or hogwash-worthy.

 

Thanks,

Bob K.

 

 



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




***** Please note that my E-Mail address has changed *****
Please address mail to me using our new [log in to unmask] address.
____________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please visit http://www.symanteccloud.com
____________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2