Les,
The problem with TDR is that everyone has a good P/T but can't correlate to
anyone else.
My search for a non destructive method of checking dielectric spacing is to
find
a mechanical way to measure impedance.
I am only concerned with trace perimeter and dielectric thickness. Dk is
more
difficult to measure and I hoped I could make it a constant at the nominal
impedance value we fix and the construction we specify. I know we are not
the
PCB experts, but the tolerances are so tight that we need at least to create
a
consensus from the PCB manufacturers for construction.
Is there any hope here or am I just wasting my time?
Thanks for all the responses on this.
Steve
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|