TECHNET Archives

June 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Barry Gallegos <[log in to unmask]>
Date:
Thu, 8 Jun 2000 16:01:07 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Anne Ledger <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Anne Ledger <[log in to unmask]>
Parts/Attachments:
text/plain (73 lines)
Barry,

Years back when the water-soluble fluxes first appeared, many
of the local assembly people experienced this white-ish 
discoloration.  After some testing, we found that the thermal
cure soldermasks (we used HySol SR series) was not 
compatible.  We switched the customer to LPI soldermask,
a semi-matte finish and the residue disappeared.  Might
be too late for your product now, but might help in the
future.

Anne Ledger
EMDS, Inc
[log in to unmask]


> -----Original Message-----
> From: Barry Gallegos [SMTP:[log in to unmask]]
> Sent: Thursday, June 08, 2000 2:14 PM
> To:   [log in to unmask]
> Subject:      [TN] Laminate condition
> 
> Dear Sirs, Madams, Guru's.
> 
>  
> 
> I have an assembly that we processed thru SMT and then thru the wave
> solder operations. Wave solder flux was with Alpha metals 856
> water-soluble. The assembly is exhibiting a white cloudy / milky
> appearance that looks almost as if the laminate/solder mask has
> changed color. No matter how much we wash this assembly, it will not
> go away.
> 
>  
> 
> Is this due to possible moisture in, around or under the solder mask /
> laminate. What is it and  is it acceptable.
> 
>  
> 
> 
> Any advice would be appreciated.
> 
> 
> 
> 
> Yours truly, (wana-be guru.)
> 
>  
> 
> Barry Gallegos
> 
> Western Electronics.
> 
> 208-377-1557
> 
>  
> 

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2