Hi TechNet's,
I wish to present you a problem that is not exactly typical to the PCB fabrication industry but I hope that it will be intellectually stimulating after all.
One of my customers wishes to make cable terminations out of brass (~1.5mm) that need to be fixed to their place by a crimping tool. His additional request is that these terminations will be covered by an insulating material.
The general idea is to bond some kind of plastic sheet (in a similar way to multilayer lamination) and then go through the punching, and forming of the cable terminations out of the brass sheet). Eventually, these terminations will be closed using the crimping tool, forming approx. a 1.5 mm radius bending of the material.
I was considering the use of a Kapton sheet or some kind of a thermoplastic material.
Does any of you have any experience with a kind of request like that. Would anyone dare offering me any ideas to try, based on his/her experience in the field of PCB production ?
All the best,
Yehuda Weisz
*************************************
* Yehuda E. Weisz
* e-mail: [log in to unmask]
* Tel: 972-3-6342045
************************************
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|