FR-4 is the flame retarded version of G-10. 
The properties may not be exactly the same
G 10 is hard to get. Nearly all epoxy laminate is FR4.
I've seen cases where the user wanted the flamibility of G-10
Better contact your customer and get the print changed, or get G-10 if you
can
J S Sallo
Sallo Consulting Services
Phone or Fax 760 346 6717.


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2