We are just starting out in Select soldering here- running about six months. I am interested in what other user's have done to qualify and develop the select solder process parameters. We've got an Ersa machine here- no problem with the machine but want to optimize the process).
I don't have the luxury of running production boards to determine the optimum machine parameters to reduce defects (i.e. insufficient solder, solder skips, insufficient topside flow). I was wondering if anyone knew of a commercially available mixed technology test board ( bottom side SMT parts and through hole devices) to run a Design of Experiments. The machine parameters I was going to look at are below:
Selective solder Design of Experiment
Variables
1. Solder pot temp (3 levels)
2. Solder nozzle height to pin Z distance (2 levels)
3. Solder nozzle X/Y speed (3 levels)
4. Z axis speed (2 levels)
5. Flux amount (2 levels)
6. Length of solder tail- max length of continuous solder path without solder dwell(control this by having several start/stop while running a single pass).
7. Lead Length (2 levels)
Noise
1. Lead length versus solder mask clearance/pitch
2. Solder mask type (dry film vs. LPI)
3. Nitrogen purity
4. Board finish (HASL vs. ENIG vs. OSP)
5. Flux type
6. Nozzle wettability
7. Nozzle calibration/axis repeatability
Any assistance or lessons learned would be appreciated.
Best Regards
Tom Gervascio
Staff Manufacturing Engineer- Automated Processes
Lockheed Martin
Ocala Operations
352-687-5442
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|