TECHNET Archives

October 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 31 Oct 2000 11:55:14 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (35 lines)
In a message dated 10/31/0 4:12:07, [log in to unmask] writes:
> One partly poor wetting component  after wave soldering, through-hole
>solder joint shows good wetting near top side PCB, but show bad wetting
>on the bottom side and through-hole is about 70% filled. some suggest good
>wetting is key to evaluate a SJ reliability. IPC suggest 75% filled is
>OK, which one I choose?
>Same situation happen to  paste in hole process, Which type SJ is ok?
>the key is the fill ratio or the good wetting?
>If half of through hole SJ is good wetting, half of which is bad, Is it ok?

Hi Liu,
Good wetting is by far the more important physical aspect--however, an
incomplete fill may be a sign of wetting problems. Further, if you have
"partly poor wetting", how do you know the rest is "good wetting"?
If you have good wetting, a partial hole fill is only important in a severe
use environment, e.g. automotive, because of the stress concentration on the
PTH barrel at the solder/no-solder interface.

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2