We use carbon ink on areas of our PWBs.  We have a question about coverage. 
 What is a reasonable expectation for coverage?  100%, 95%, all but  the 
very edges of a pad?

We are seeing on touch pads slivers on the edges that are not covered with 
carbon ink.  Is this a problem?  If it is a problem, how can our supplier 
fix the process?

Marti Tully Sr. SQE Honeywell IAC
602 313-3346
[log in to unmask]

Gary Seppanen
602 313-3175
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2