TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Long, Thomas" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 26 Oct 2001 13:47:56 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (31 lines)
        As a follow up to an earlier e-mail regarding a corrosion issue on
two Aqueous Technologies DI cleaners, it appears it was an isolated vendor
issue supplying the heaters.  Most likely the heater fins were not cleaned
prior to coating application.  Aqueous has taken steps to ensure proper
coating adhesion in the future, and has promised to replace anyone's heater
coils that is  experiencing heater coil issues with the new improved
product.  I am glad this was brought to closure quickly as the machines have
performed well for us in general.

                        Tom Long

************************************
If this email is not intended for you, or you are not responsible for the
delivery of this message to the addressee, please note that this message may
contain ITT Privileged/Proprietary Information.  In such a case, you may not
copy or deliver this message to anyone.  You should destroy this message and
kindly notify the sender by reply email.  Information contained in this
message that does not relate to the business of ITT is neither endorsed by
nor attributable to ITT.
************************************

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2