TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Lautaro Gutierrez <[log in to unmask]>
Date:
Thu, 27 May 1999 20:32:58 -0700
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"\"TechNet E-Mail Forum.\" <[log in to unmask]>, Lautaro Gutierrez" <[log in to unmask]>
Parts/Attachments:
text/plain (139 lines)
--- Roger Massey-G14195 <[log in to unmask]> wrote:
>      Lautaro,
>
>         There are a number of "methods" (over 30
> reported) for measuring
>      the hardness of materials, of which Shore is
> only one!
>
>         From what I understand, the Shore method
> makes use of a
>      scleromoter.  Basically, a small diamond
> pointed hammer weighing 2.5g
>      is allowed to free fall 250mm down a glass tube
> (graduated into 140
>      parts) The hardness is related to how far back
> the hammer rebounds
>      after its first rebound off the material
> sample. ASTM E448 has the
>      basic outline for the methodology, so I would
> take a look at that if
>      you are planning on using Shore tests
>
>         Other common methods include
>
>         Brinell - a 10mm steel ball is pushed into
> the sample with a set
>                 load and time, hardness is related
> to the size of the mark
>                 left in the sample. Not very good
> for very hard materials
>                 See ASTM E10
>         Vickers - Diamond tipped, square based
> pyramid pushed into the
>                 sample, again hardness relates to
> the size and shape of the
>                 mark left behind.  See ASTM E92
>         Rockwell - uses either a 1.58mm ball @ 100Kg
> (Scale B) or a diamond
>                 cone @ 150Kg (Scale C) this time the
> output dial indictaes
>                 depth of penetration which can be
> converted to an
>                 indication of hardness. See ASTM E18
>
>         Microhardness machines are used where the
> sample is either very
>      thin such as platings or very soft and is often
> based on the Vickers
>      or Knoop methods, See ASTM E384
>
>                 Good Luck,
>
>
>
>      Roger
>
> ______________________________ Reply Separator
> _________________________________
> Subject: [TN] Shore hardness
> Author:  "TechNet E-Mail Forum." <[log in to unmask]>
> at #email
> Date:    25/05/99 19:53
>
>
> Please, send my a message if you know how does the
> shore harness method
> works. I need inmformation urgent!
> I must do a work: harness of different materials,
> any idea?
>   Thanks!!!!
>
> _________________________________________________________
> Do You Yahoo!?
> Get your free @yahoo.com address at
> http://mail.yahoo.com
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by
> IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to
> [log in to unmask] with following text
> in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org)
> "On-Line Services" section for
> additional information.
> For technical support contact Hugo Scaramuzza at
> [log in to unmask] or 847-509-9700
> ext.312
> ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by
> IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to
> [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org)
> "On-Line Services" section for additional
> information.
> For technical support contact Hugo Scaramuzza at
> [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>
>

_________________________________________________________
Do You Yahoo!?
Get your free @yahoo.com address at http://mail.yahoo.com

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2