The temperature profile of the board during baking should exceed the Tg by
at least 3 degrees for 10 to 20 minutes but that also depends on the amount
of weight applied.


Etgar D.

----------
> From: Ashok Tiwari <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] PCB Baking
> Date: Tuesday, March 23, 1999 2:07 AM
>
>  Hi Technetters,
>
> Is any body there who can tell about the baking process ( time &
> temperature) to remove the warpage in the bare PCB ?
>
>
> Thanks,
>
> Ashok
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2