Hi Yehuda,
A more than complete specification of the HASL finishing is at http://people.ne.mediaone.net/sgoodell/chapter30/ch30.html
It's a complete chapter of the "Printed Circuits Materials Handbook".
Kind regards,
Daan Terstegge
Unclassified mail
Personal Website: http://www.smtinfo.net
>>> Franklin D Asbell <[log in to unmask]> 02/20 11:19 pm >>>
Yehuda,
After your first reflow cycle the original solder thickness is
unimportant...
Thickness will also not be a major contributor to shelf-life...what
would affect this is the quality of the solder coating...
Most HASL processes should be able to produce acceptable solderability
up to a year after fabrication provided they are package accordingly,
and stored in an decent storage facility (average temperature/humidity).
My suggestion would be to state the quality level you expect, at
receiving, after 6 months, a year, etc, etc. Writing a requirement for
continued solderability up to and beyond 3 thermal cycles may be a bit
much, unless you're able to work well with the supplier...
My $12.00 worth ~my time is more expensive then a mere two cents
~grins~~
Franklin D Asbell
> Yehuda Weisz wrote:
>
> Dear Technetters,
> I am trying to write a spec. for solder levelled boards received from
> an outside vendor. The boards contain SMD (some - 0.019" pitch) and
> some pressfit connectors.
> What solder thickness should I ask for if I wish the boards to
> maintain solderability after at least one year of storage (under
> normal conditions) and 3 reflow assembly cycles (sometimes even more).
>
> Probably, all of you had seen specs that made no sense, I don't want
> to write another one.
>
> I'll appreciate very much your inputs.
>
> Yours,
> Yehuda Weisz
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|