Carrie,
Other things to consider:
1. How deep the cut, does it get into internal layers?
2. How long is the cut?
3. Is their any high voltage?
4. Is any copper exposed after cut?
I typically coat everything, less chance of problems later!
I agree spec should read, "AS"
Tom B.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Morse, Carrie
Sent: Tuesday, January 20, 2004 1:15 PM
To: [log in to unmask]
Subject: [TN] Conductor Cuts -- Question about using Epoxy
This question goes out to all those Repair Guru's:
Paragraph 8 of Procedure 4.3.1 of IPC 7721A (Repair Guide) states "Coat the
area with epoxy IF needed".
Is that "IF" part correct?. If so, what does "IF" mean. Should that say
"AS" needed? Or...are we actually given the option as far as using epoxy?
-Carrie
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|