Many newer wave-solder and selective solder machines have a titanium-lined pot and/or sump. The newer the machine, the higher the Ti count.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
Sent: Thursday, June 13, 2013 9:04 AM
To: [log in to unmask]
Subject: [TN] Titanium
Dear Technetters,
We are seeing some titanium residues (confirmed by EDX) on solder joints after wave soldering post wash (that is not to say they are not present post wave, more analysis is ongoing). Water soluble process, high lead alloy, and a saponified wash. So far the Ti residues are only detectable on the solder joints, not on the assy surface. For general information. what are some possible sources of Ti on the assembly?
Regards,
Amol
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|