For this insertion, was it by hand followed by an arbor press or was it
machine placement/insertion? What was the failure mechansim?
Doug Pauls
Rockwell Collins
"Fox, Ian" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
06/11/2009 02:12 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Fox, Ian" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Conformal Coat and Compliant Pins
Doug, we tried to do this when we first started down the press-fit route
but we found issues with coating (acrylic) build-up in holes preventing
proper insertion so now we insert first then coat
Regards
Ian Fox
Lead Materials and Process Engineer
Aero Engine Controls
A Rolls-Royce plc and Goodrich Corporation Joint Venture
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: 10 June 2009 20:59
To: [log in to unmask]
Subject: [TN] Conformal Coat and Compliant Pins
Good afternoon all,
Some questions came up here in a conversation this morning and I wanted
to ping the Technet group on the topic.
Do you know of papers that have been published on the topic of inserting
compliant pin / press-fit pin connectors on a conformally coated
assembly?
Do any of you do this routinely? If so, what are the benefits and
disadvantages.
Thanks in Advance.
Doug Pauls
Rockwell Collins
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
--------------------------------------------------------------------------
This message (and any attachment) is confidential and is intended for the
named recipient only.
If you receive it in error please e-mail back the sender and permanently
delete the original message and any copies.
Rolls-Royce Goodrich Engine Control Systems Limited.
Registered Office: Moor Lane, PO Box 31, Derby, DE24 8BJ.
Registered in England No. 06686268.
--------------------------------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|