Hi Bev
If it's your design (I'm assuming so) then you can do whatever you want to put on a drawing. However - there are no inspection criteria for an intentional solder bridge. How do you define how much solder to use?
We would use a mod wire so as to ensure a consistent mod, but I guess it depends on the criticality of the application.
regards,
Graham Collins
Process Engineer,
Northrop Grumman Canada Corporation
Halifax
(902) 873-2000 ext 6215
>>> [log in to unmask] 01/16/03 03:01PM >>>
Technetters,
How do I do what is proposed in my title? The options are using excess solder or using a mod wire. Are there other options for doing this mod? What do people do? What is allowed and not allowed by IPC standards (I couldn't find anything, but then I may not be looking in the right place.) I would expect option one would be a whole heck of a lot easier than option 2. As long as option 1 doesn't produce bulbous joints with the solder all the way up to the component body is there any real reason why I can't do this?
regards,
Bev Christian
Research in Motion
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|