We saw this in early testing of Pb-Free solder. Solder would climb the leg
up to the package.
But, then drop back down as the surface tension and wetting forces
equalized.
This looks like something inhibited that phase of the reaction.
I wonder if Wayne isn't on to something. The solder looks doped.
Guy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jerry Dengler
Sent: Monday, June 28, 2010 7:40 AM
To: [log in to unmask]
Subject: Re: [TN] QFP short at top of the leads
Jowan,
Was this part dipped in solder before placing? It looks like solder has
coated the whole lead right up to the body.
Jerry
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Iven, Jowan
Sent: Monday, June 28, 2010 5:08 AM
To: [log in to unmask]
Subject: [TN] QFP short at top of the leads
Has anyone ever seen a QFP where shorts occur after soldering at the top
of the leads?
And the leads look pretty dull after soldering. Any ideas?
A picture is available at
http://ipc-technet.groupsite.com/uploads/galleries/x/000/020/5ba/technet
01.jpg
Jowan Iven
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|