TECHNET Archives

May 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Graham Naisbitt <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Date:
Thu, 12 May 2016 11:58:07 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (54 lines)
…and to back-up what Dave reports, please note that ALL the test fluxes for J-STD-002 and 003 were originally developed by Multicore.

We still make these named with both the original SMNA - Actiec 2 = IPC Flux #1 and Actiec 5 = IPC Flux #2

I mention this because we continue to have a large number of users who still order Actiec Fluxes in place of the IPC variants.

Also for all you history buffs, the original pure W/W Rosin SMNA, after an investigation that would have foxed Sherlock Holmes, is derived from SMYRNA, in old Anatolia, Izmir today. The pine trees produced an excellent resin with great consistency from season to season.

Sorry for any commercialism, but I was feeling left out….

Graham N

> On 11 May 2016, at 13:33, David Hillman <[log in to unmask]> wrote:
> 
> Hi Victor - if you are conducting solderability test per either the IPC-
> JSTD -002 or -003, the fluxes specified for testing are listed in one of
> the Appendices by product name/supplier. The specifications also list the
> flux chemistry constituents so that you can mix it yourself. One word of
> caution -there are dozens of ROL1 fluxes on the market but they do not meet
> the requirements of the JSTD specifications.
> 
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
> 
> On Wed, May 11, 2016 at 7:26 AM, Victor Hernandez <
> [log in to unmask]> wrote:
> 
>> Fellow TechNetters:
>> 
>>   Does anyone out there have a part number for the above solder type.
>> Need to conduct bare board solder float test, 1x. 3x and 6x.   Ten second
>> intervals.
>> 
>> Victor,
>> 
>> 
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>> 
> 
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2