In a former life (Commercial Avionics/Military Avionics) we tried using LCCC's with miserable results. We used them on FR4 and Teflon PCB's. After only several hundred temperature cycles (-55C to 85C @ < 5C/min), the solder joints would crack. We stopped using them as fast as we could get new parts spec'ed and PCB's relayed out for compliant pin packages.
Brent
Reliability/Quality Engineer
>>> [log in to unmask] 07/20/00 11:35AM >>>
Greetings,
Is anybody out there using leadless ceramic chip carriers in a military environment without attaching leads? If so, what size are you using?
Thanks in advance for any information,
Bill Robinson
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|