TECHNET Archives

January 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Christopher Jorgensen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 8 Jan 1999 09:24:05 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (58 lines)
Edwin,

Larry Johnson at GE Coshocton would be able to provide you with information on Getek.
He can be reached at 740-623-6327 or e-mailed to [log in to unmask]

Chris

Chris Jorgensen
Project Manager
IPC
2215 Sanders Rd
Northbrook, IL 60062
-p- 847-509-9700 x. 5328
-f- 847-509-9798
[log in to unmask]

>>> Edwin Maximo <[log in to unmask]> 01/07/99 04:23AM >>>
Hi there,

We will be conducting an evaluation on Getek and BT boards for one of
our customers. This will be the first time for us to assemble
components on a GEtek board, is there anyone out there who has
experience or had a knowledge about Getek boards. What considerations
should we have to look at e.g. profile for reflow, are there any
difference between a BT board and a Getek board?
Any information you could render will be appreciated.

Regards,
Edwin Maximo
Value Engineer
Electronic Assemblies Inc.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2