Rainer,
Thanks for the input. I had mentioned that process as a possibility to my
engineers but have not tried it yet. I am glad that someone has seen it
work. I don't currently have a wave solder so I would still have to hand
solder but the solder mask would keep solder off the pins in either process.
Joel
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blomberg, Rainer (FL51)
Sent: Tuesday, October 04, 2005 9:43 AM
To: [log in to unmask]
Subject: Re: [TN] Hand Soldering Long Gold Pins
We had a similar situation with a 4-row connector with 1" long gold pins.
The process solution was to dip the pin array into a trough of latex solder
mask to the desired depth and cure. We then ran the boards through wave
soldering and mechanically peeled the rubbery latex off the pins revealing
clean, unsoldered gold surfaces.
> Rainer G. Blomberg
> Staff Production Engineer
> Space Systems - Clearwater
> Honeywell International, Inc.
> * Phone (727) 539-5534
> * Fax (727) 539-4469
> * Email [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joel Mearig
Sent: Tuesday, October 04, 2005 11:59 AM
To: [log in to unmask]
Subject: [TN] Hand Soldering Long Gold Pins
I have a number of assemblies that have long (0.5") connector pins that must
be soldered in the board. The pins must remain gold so at the moment I am
trying to hand solder. This is a difficult process. The 0.100" spacing makes
it difficult for my production personnel to solder without getting solder on
the gold pins.
The connectors are double row and there are two beside one another creating
a four pin bank of 0.100" spaced pins. Any thoughts on how I can improve
this process for the soldering personnel would be greatly appreciated.
Joel Mearig
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|