Yes OSP is used on Automotive products - Delphi has for years run OSP on all
types of modules found in the car including ECM's under hood.
If you mean electrolytic plated gold then the color will be a function of
deposit thickness, quality of the gold bath, ASF used to plate, impurities
in the bath, the amount of Nickel deposited and more importantly the surface
preparation of the underlying copper.
I am not aware of any such color shade chart.
Regards
Gerard O'Brien
Photocircuits Corporation
Co-Chairman of 4-14 plating subcommittee on surface finish.
-----Original Message-----
From: Janoch Jirí, Ing. [mailto:[log in to unmask]]
Sent: Thursday, October 14, 2004 1:19 AM
To: [log in to unmask]
Subject: [TN] OSP and Gold
Hi Techneters,
I've got some questions, please .
1. Does anybody use OSP on PCB for automotive assemblies and is it
reliable enough ?
2. Can the galvanic gold-plated pads have different colour shade
from various manufacturers and is the gold-colour shade important for
the proper contact ?
3. Is there any note of gold-colour shade in the IPC standards ?
4.
Very thanks for answers
J.Janoch. TSE
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|