TECHNET Archives

October 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 30 Oct 2000 17:36:11 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (46 lines)
It's a little confusing...but then I'm not the expert.

In regards to exposed vias...the artwork will dictate what vias are to
be exposed and/or plugged so the mention of that in the notes may
confuse the issue. Stating Green LPI IAW SM-840 should be enough in most
cases I would suspect. Your comment on 'associated vias'...what exactly
are 'associated vias? Is this all vias on a commen net?

Hope the critique helps some.

Franklin



Ken Patel wrote:
>
>         Fab Expert,
>         Is the following fab note make sense to you or should I also mention
> the plugging side as I do not want higher surface on fine-pitch side. Also,
> comment on use of SR1000 epoxy in my fab note.
>
>         SOLDERMASK: GREEN PHOTOIMAGEABLE, BOTH SIDES PER IPC-SM-840, CLASS
> 3. ALL TEST-VIAS AND ASSOCIATED PADS ARE TO BE FREE OF SOLDERMASK. ALL
> NON-TEST VIA HOLES TO BE PLUGGED WITH SR1000 OR EQUIVALENT EPOXY.
>
> re,
> ken patel
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2