"<Peter George Duncan>" <[log in to unmask]>
Date:
Mon, 19 Nov 2001 11:30:21 +0800
Content-type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (235 lines)
Thanks for your advice, Roger. I have looked into this already, but the
spacing available on the over-etched area isn't enough to widen the pads by
the 4 mils or so needed without winding up with a solid copper strip.

Will continue the quest!

Best regards

Peter Duncan




                    "Roger M. Stoops"
                    <rstoops@SPECTRAPRECISI        To:     [log in to unmask]
                    ONDAY.COM>                     cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    Sent by: TechNet               Aero/ST Group)
                    <[log in to unmask]>              Subject:     Re: [TN] Over-etch


                    11/16/01 11:28 PM
                    Please respond to
                    "TechNet E-Mail Forum."






Peter,
I'm probably out of my league here, but the board house may be able to
compensate somewhat with "etch compensation", adding copper width where the
most etching will take place.  If you know you're going to lose 2 or 3 mils
[.05-.08mm] per side in the final etch, add on copper before the
lam/drill/plate processes to get what you want.  Check with your supplier
to see if this would work.  I know this doesn't help you with this board
now, but may fix future problems.  Time for Tums...(or Rolaids, Ativan,
Guinness, etc.).
Roger M. Stoops, C.I.D., PCB Designer
[log in to unmask]


Trimble
Engineering and Construction Division
5475 Kellenburger Rd.
Dayton, OH 45424-1099 USA
Ph: +01 937.233.8921 or +01 937.233.4574 ext 288
Fax: +01 937.233.7511



                    "<Peter
                    George               To:     [log in to unmask]
                    Duncan>"             cc:
                    Sent by:             Subject:     Re: [TN] Over-etch
                    TechNet
                    <[log in to unmask]
                    ORG>


                    11/16/01
                    03:04 AM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum."





Hi, Rudy,

The boards are ENIG finished, the ENIG plating being carried out
post-solder-mask, which must be after final copper etch, so No, there is no
other metal in the area, unless my understanding of the plating/etching
sequence is all wrong. My understanding (faulty or otherwise) of what the
fab house has done, is that they laminate, drill and plate the layers with
the  first suite of blind vias, then laminate, drill and plate for the
second suite of blind vias, then again for the 3rd suite until everything
is stacked up, pressed, drilled and plated for the through-holes. I haven't
quite been able to make sense of it all yet, but I think what I'm being
told is that the plating becomes "stepped" somehow. I have 3 sets of blind
vias from each outer surface (for ease of argument), making 4 plating
sessions on each side by the time the through-hole group is done. The first
areas to be drilled and plated are therefore plated 4 times, while the last
areas to be drilled are only plated once, with the groups in between
getting their proportional share of multiple plating.

Thus at final etch, there is, I am told, a compromise to be reached - how
to achieve the correct widths and spacings on the heavily plated areas
without over-etching the lightly-plated areas. In my simple way, I would
have expected the entire board surface to have an even plating thickness,
however thick, but seemingly not. The compromise hasn't worked for the
number of blind via groups featured in this board, and I need to try to
find out how to address a solution without solely relying on what our fab
house tells me.

In my entire life, I never had to worry about the processes involved in
fabricating PCB's - only that components could be soldered to them, that
they passed test and proved to be reliable in the field. I only ever worked
with good boards - the ones that passed in-coming inspection - in an
assembly environment, so my experience of board design and PCB fab is
limited to the past 8 or 9 months, in a company that has no previous
convictions for designing this type of board, so it's a case of the blind
leading the blind to a certain extent.

Any further help in this area would be greatly appreciated.

Best regards

Peter Duncan




                    "<Rudy
                    Sedlak>"             To:     [log in to unmask]
                    Sent by:             cc:     (bcc: DUNCAN Peter/Asst
Prin Engr/ST
                    TechNet              Aero/ST Group)
                    <[log in to unmask]        Subject:     Re: [TN] Over-etch
                    ORG>


                    11/16/01
                    02:13 PM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum."






Peter:

I am not sure if I fully understand the process you are using....so I am
going to ask a dumb question, that may shed some light on the issue...

Is there, anywhere in electrical contact with Copper being etched any other
metal excepting Tin?

This sort of thing, selective over-etch, is classically seen when there is
some other metal, (Nickel, Gold, or???) than Tin in electrical contact with
the over-etched Copper, and also in contact with the etchant.

And if I am completely out in space with this question, please forgive the
intrusion.

Rudy Sedlak

---------------------------------------------------------------------------------



Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------







[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------


Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------


---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2