TECHNET Archives

January 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Marsico, James" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 24 Jan 2002 16:20:16 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (131 lines)
Thanks Mike, this sounds like a good idea.  One question though, when do you
remove the mask, before or after cure?  If before, doesn't the coating run
when heated?  If after, how do you separate the tool from the coating?  (OK,
three questions)

Thanks again,
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879


        -----Original Message-----
        From:   Michael Bell [SMTP:[log in to unmask]]
        Sent:   Thursday, January 24, 2002 2:05 PM
        To:     [log in to unmask]
        Subject:        Re: [TN] Masking for Conformal Coating

        James,

        Have you considered using a laser cut or milled steel/aluminium hat
that
        sits ontop of the PCB.  Any clearance for components can be milled
out from
        the underside, and the weight of it forms a good enough seal around
the
        bottom.  We used this idea ffor a long time for PCB's that were
panelized.
        The hats were made into a large spider web style with hats
adjointing to it.
        You simply dropped it over the respective components and in one go,
we
        masked about 30 components/connectors etc.

        Cheers

        Mike

        -----Original Message-----
        From: Marsico, James [mailto:[log in to unmask]]
        Sent: Friday, 25 January 2002 05:24
        To: [log in to unmask]
        Subject: [TN] Masking for Conformal Coating


        Hello again...

        Looking for suggestions for removing masking material (tape or
liquid) which
        is applied to mask areas from conformal coating.  The way we do it
now, the
        operator masks off the area (usually tape), sprays the board, cures
the
        coating, scores the coating around the tape, then removes the tape.
We're
        trying to eliminate the scoring of the coating since this has
potential of
        cutting through traces.  Removal of the coating prior to curing
doesn't work
        because the coating runs during the heat cure process.  I'm trying
to avoid
        room temperature cure since this is very time consuming.  Ant
suggestions?

        Jim Marsico
        Senior Engineer
        Production Engineering
        EDO Electronics Systems Group
        [log in to unmask] <mailto:[log in to unmask]>
        631-595-5879


----------------------------------------------------------------------------
        -----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send e-mail to
[log in to unmask]: SET
        Technet NOMAIL
        To receive ONE mailing per day of all the posts: send e-mail to
        [log in to unmask]: SET Technet Digest
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
        E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
        ext.5315

----------------------------------------------------------------------------
        -----


----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2