Pb-Free Loctite 3508
-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Tuesday, December 09, 2014 4:08 PM
To: 'TechNet E-Mail Forum'; 'David Hillman'
Subject: RE: [TN] BGA Reflow Issue
Loctite makes a BGA corner bonder that allow the balls to melt then cures. And it is reworkable.
For SnPb it is Loctite 3515. I don't remember the Pb-Free part number.
Guy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman
Sent: Tuesday, December 09, 2014 3:47 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Reflow Issue
Hi Ioan! Yep, its falling off as we have had a couple of them stay in the reflow oven for some additional "hot" time! A good friend and TechNet lurker, Fritz Byle of Astronautics, made me a Excel program many years ago that calculates & compares BGA weight to surface tension so I can usually predict if I am going to have a problem. This BGA in question is one of those that is "right on the edge of the cliff" in terms of holding on. We have looked at reflow profile changes but I just can't convince the Laws of Physics to temporarily go away for the BGA so I am working "Plan B" with the temporary mask material until we can revise the assembly and move the BGA to process side two.
Dave
On Tue, Dec 9, 2014 at 2:11 PM, Ioan TEMPEA <[log in to unmask]>
wrote:
> Hi Dave,
>
> Just out of curiosity, have you seen the BGA falling or you are just
> afraid it might?
>
> Because I have ran thousands of BGAs in second reflow (ceramic, metal
> top, name it), on bottom side, with absolutely no BGA loss. The balls
> would keep their collapsed aspect, even though they might be slightly
> stretched, but this is bound to improve compliance, hence long term reliability.
>
> Best regards,
>
> Ioan Tempea
> MDA Corporation
> >
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman
> > Sent: Tuesday, December 09, 2014 8:42 AM
> > To: [log in to unmask]
> > Subject: [TN] BGA Reflow Issue
> >
> > Hi gang - looking for an adhesive suggestion. I have an assembly in
> > which a heavy BGA was accidently located on process side one
> > (bottom) so that when we reflow process side two (top) the BGA is
> > doing its best to fall off.
> > Unfortunately I can't reverse my process order for a couple of
> > reasons so I am looking for a temporary fix until I can get the
> > assembly revised. I was thinking of using some type of adhesive to
> > temporarily hold the BGA in place during reflow - tack down the
> > corners sort of action. Does anyone have any adhesive (ideally
> > temporary, water
> > washable/removable) suggestions I can investigate?
> >
> > TIA
> >
> > Dave Hillman
> > Rockwell Collins
> > [log in to unmask]
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|