TECHNET Archives

June 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ian Hanna <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ian Hanna <[log in to unmask]>
Date:
Fri, 18 Jun 2010 12:36:13 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (209 lines)
IPC 6012 3.3.9 Workmanship 'boards shall be processed in such a manner
as to be uniform in quality and show no visual evidence of dirt foreign
matter, oil, fingerprints....that affect life, ability to assemble and
serviceability.' I

If it will cause a problem, then it is a problem.
If it will not cause a problem, then it is not a problem.

Simple...



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Linda Langley
Sent: Friday, June 18, 2010 12:20 PM
To: [log in to unmask]
Subject: Re: [TN] 3M tape/adhesive concern

Does anyone know if this would be a defect per IPC?

Linda Langley CIT
Training Specialist
Jabil Circuit
248-292-6176
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, June 17, 2010 8:38 AM
To: [log in to unmask]
Subject: Re: [TN] 3M tape/adhesive concern

Hi Linda!

 

Gosh, I'm sorry I didn't get these posted earlier. I was planning to as
soon
as I got them, but I got busy doing something else and forgot about your
request. Thanks for reminding me.

 

Anyways, here's your pictures:

 

http://stevezeva.homestead.com/adhesive.JPG

 

http://stevezeva.homestead.com/adhesive_2.JPG

 

http://stevezeva.homestead.com/paper_debri.JPG

 

http://stevezeva.homestead.com/under_button.JPG

 

I know it's bit of a challenge to find good conformal coat masking tape
that
doesn't leave residues and debris, especially if you bake the boards to
tack
cure the coating.

 

I don't know why Humiseal quit making their tape, it was one of the best
tapes I ever used. But then they just stopped making it for some reason.

 

Steve

 

From: Linda Langley [mailto:[log in to unmask]] 
Sent: Monday, June 14, 2010 2:43 PM
To: Steve Gregory
Subject: FW: 3M tape/adhesive concern

 

Steve,

Could you please post these pictures? We are having problems where there
is
adhesive is sticking to the board when we pull the tape off.

Does anyone know if this would be a problem according to IPC? Would this
be
considered Particulate Matter? Any info will be greatly appreciated.

 

Thanks

 

Linda Langley CIT

Training Specialist

Jabil Circuit

248-292-6176

From: Klara Szalay 
Sent: Tuesday, June 08, 2010 8:23 AM
To: Linda Langley
Subject: RE: 3M tape

 

I am sorry, I had to leave early yesterday. Here are some pictures of
what
you looked at yesterday. Let me know if you need additional pictures.

Klara

 

From: Linda Langley 
Sent: Monday, June 07, 2010 10:37 AM
To: Klara Szalay
Subject: 3M tape

 

Klara,

Can you send me a picture of the tape concern?

 

Linda Langley CIT

Training Specialist

Jabil Circuit

248-292-6176



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2