TECHNET Archives

May 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Matthias Mansfeld <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Matthias Mansfeld <[log in to unmask]>
Date:
Fri, 20 May 2016 23:17:11 +0300
Content-Type:
text/plain
Parts/Attachments:
text/plain (32 lines)
On 20 May 2016 at 18:08, stephen gregory wrote:

> Hi All, Question, how common is the practice of using high current
> to clear bare PCB inner layer shorts? 

Concerning my customers and suppliers: forbidden, because the remains 
of the "fired" short (charred board material, "doped" with finespread 
copper) end up (depends on the normal operation voltages between 
these tracks) with slow "dendrite" growth and subsequent new shorts. 
In the best case the unit fails completely, in the worst case, the 
new, fine dendrite structures get blown with contact, cause a 
sporadic error (reboot or something else) and the game begins new. 
Sporadic fail every X hours (the time the blown dendrite needs to 
grow again).

Regards
Matthias Mansfeld
--
Unsere Korrespondenz kann mitgelesen werden. Wollen Sie das 
erschweren, mailen wir uns gerne mit (Open)PGP verschlüsselt.
-
Matthias Mansfeld Elektronik * Leiterplattenlayout
Neithardtstr. 3, 85540 Haar; Tel.: 089/4620 093-7, Fax: -8
Internet: http://www.mansfeld-elektronik.de
OpenPGP: http://www.mansfeld-elektronik.de/gnupgkey/mansfeld.asc
Fingerprint: 6563 057D E6B8 9105 1CE4 18D0 4056 1F54 8B59 40EF

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2