TECHNET Archives

November 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 29 Nov 2010 16:50:39 -0500
Reply-To:
Bob Landman <[log in to unmask]>
Subject:
From:
Bob Landman <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (83 lines)
Ioan,

Have you seen this paper on the use of ACF for displays?

http://www.tju-hj.com/publication/Bonding%20Parameters%20of%20Anisotropic%20Conductive%20Adhesive%20Film%20and%20Peeling%20Strength.pdf

Bob Landman
H&L Instruments,LLC
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Monday, November 29, 2010 1:32 PM
To: [log in to unmask]
Subject: [TN] Cleaning of ACF bonder

Dear Technos,

 

We need to clean the ACF bonder from a fair quantity of boards (about 1K/ month). The material to clean is Hitachi Anisolm, per the specification below (unfortunately there's not much in this spec)

http://lituo.testmart.cn/Images/UpLoadForderElse/2009_12_30_13_38_38_4939.pdf <http://lituo.testmart.cn/Images/UpLoadForderElse/2009_12_30_13_38_38_4939.pdf> 

 

We have been suggested to use a 48 hour soak in 1-Methyl-2-Pyrrolidinone, followed by an acetone cleaning. It is only the bonding contacts that are immersed in the methyl-pyrr..., but the level of substance is only 2 mm away from an overmolded die-attach. The acetone cleaning is local on the contacts.

 

First question would be: are the above chemicals OK for this usage? Board is FR4, with gold-plated contacts.

 

Second question would be: what else could we use to remove the bonder? Manufacturer seems to recommend Dow Corning OS-20, but we were told by our customers it does not exactly work.

 

Thanks,

 

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer T | 450.967.7100 ext.244 E | [log in to unmask] <mailto:[log in to unmask]> W | www.digico.cc <http://www.digico.cc/> 

 
 N'imprimer que si nécessaire - Print only if you must

 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2