TECHNET Archives

September 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jerry Dengler <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jerry Dengler <[log in to unmask]>
Date:
Mon, 13 Sep 2010 09:53:21 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (210 lines)
I filled out the survey, but did not enter any contact information at
the end.  I don't care about the carrot being dangled to enter data.

Jerry Dengler

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Monday, September 13, 2010 9:48 AM
To: [log in to unmask]
Subject: Re: [TN] Chance to remain competitive and help. Your opinion
needed

No no no, you are thinking of SurveyBanana.  Many people have slipped up

on it............  some days I just slay me.

IPC has been using SurveyMonkey for some of their work and it seems to 
work pretty well.  What problems have their been?

Doug Pauls



"Stadem, Richard D." <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
09/13/2010 08:33 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Stadem, Richard D." <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Chance to remain competitive and help. Your opinion needed






I have heard of really bad experiences associated with Surveymonkey.
Stay 
as far away as possible.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Sunday, September 12, 2010 6:50 PM
To: [log in to unmask]
Subject: Re: [TN] Chance to remain competitive and help. Your opinion 
needed

Call me paranoid, but something doesn't smell right about this...

--------------------------------------------------
From: "Terry Baker" <[log in to unmask]>
Sent: Sunday, September 12, 2010 4:46 PM
To: <[log in to unmask]>
Subject: [TN] Chance to remain competitive and help. Your opinion needed

> Hello to all interested parties, I am a doctoral candidate looking for
> participants in a survey about supply chain efficiency based on
> communication. Particularly I am interested in people in the PCBA 
(Printed
> Circuit Board assembly) industry in manufacturing, sales, purchasing,
or
> operations management to give me your opinions on supply chain 
efficiency.
> Everyone who fills out the survey has a chance to win a 500 dollar
cash 
> prize,
> the odds are one in three hundred or even maybe less. The data is not
> sensitive or private in nature to your company, its based on your 
opinions
> only. There are more details at the survey link, which is data
encrypted 

> and
> secure. Please participate and help me if you can :-) Just copy and 
paste 
> this
> link, and it should take you right to the survey in Survey Monkey. I
am 
> happy
> also to provide the results of the survey to you if you wish to see
what 

> are
> competitive measures you can take in your business. You can email me
at
> [log in to unmask] if you have any questions. Thank you so much for
your
> time.
>
> https://www.surveymonkey.com/s/SupplyChainSurveySeptember2010
>
> Sincerely
> Terry Baker
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text

in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
http://listserv.ipc.org/archives
> Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at
[log in to unmask] 
or 
> 847-615-7100 ext.2815
> ----------------------------------------------------- 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2