TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Lee Parker <[log in to unmask]>
Date:
Thu, 13 Jan 2005 08:21:51 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Parts/Attachments:
text/plain (78 lines)
Hard gold is not much used in electronics. We use microhardness tester (Vicker diamond) to check in case of uncertainty. 'Ordinary' component and board gold use to be approx. 80 HV, while the hard type can be over 300 HV. Hard gold is used when the part is exposed to mechanical wear. Unfortunately, you can get unwanted impurities into the bath without knowing, resulting in a somewhat harder than normal gold.

Ingemar Hernefjord
Ericsson Microwave Systems

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]
Sent: den 12 januari 2005 18:14
To: [log in to unmask]
Subject: Re: [TN] soft vs. hard gold


Janoch

Galvanic gold is more commonly referred to as immersion gold. It is
essentially pure gold and consequently "soft".

What is referred to in the industry as hard and soft golds are usually
electroplated. If only gold is plated, it is called soft gold. When a
hardener is added as is often the case for contacts or connector fingers
the plated metal is no longer pure gold and is called hard gold.

Best regards

Lee

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Janoch Jiøí, Ing.
Sent: Wednesday, January 12, 2005 3:18 AM
To: [log in to unmask]
Subject: [TN] soft vs. hard gold

Hello Technetters,
If galvanic gold plating used, what is the difference between soft and
hard gold ?
(appearance, durability, environment resistance etc.)

Thanks for reply

J.Janoch, TSE

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2