Hi John, Ingemar,
The only way I recommend to check (first in prototypes) a pre tinning
process as follows:
1. Preform the capacitors to the final shape.
2. Assemble the capacitors on Platte of FR4 drilled to the right pitch
(without any copper plate on surface or in holes). The holes should be
about 1.5 mm greater than the capacitors leads diameter.
3. Use an aggressive flux in your wave soldering and pre heating and
soldering as usual.
4. Clean the capacitors with solvent.
5. Check the results.
Pls inform results.
Best Regards
ROKAH Reuven
"Ingemar Hernefjord
(KC/EMW)" To: [log in to unmask]
<ingemar.hernefjord@ER cc:
ICSSON.COM> Subject: Re: [TN] Question about wetting
Sent by: TechNet
<[log in to unmask]>
20/10/2003 10:05
Please respond to
"TechNet E-Mail
Forum."; Please
respond to "Ingemar
Hernefjord (KC/EMW)"
Listening with great interest. THIN layer of tin over nickel, what a
situation! If the nickel has degraded too, I just wonder how on earth it
can be restored. The guru advices are many, hope one or the other will
work. Please, let us know who got beer for the rest of his life...
Ingemar Hernefjord
Ericsson Microwave Systems
-----Original Message-----
From: John Foster [mailto:[log in to unmask]]
Sent: den 17 oktober 2003 20:14
To: [log in to unmask]
Subject: [TN] Question about wetting
I have a large inventory of trim capacitors that have exceeded the
manufacturers shelf
life by 2 years. Solderability testing has revealed inadequate wetting. The
parts are on
tape and reel. The plating is a thin layer of tin over nickel. We believe
we
have a oxidation problem. Does anyone have any ideas AT ALL on how we can
recover these
parts. The part has gone obsolete I have 86,000 of these things that I
really really need to use.
Any help would be appreciated
Thanks
John Foster
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|