TECHNET Archives

November 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Mark Austin <[log in to unmask]>
Date:
Mon, 9 Nov 1998 12:25:00 +0000
Content-Transfer-Encoding:
7BIT
Content-Type:
text/plain; charset="ISO-8859-1"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Mark Austin <[log in to unmask]>
Parts/Attachments:
text/plain (104 lines)
All

I am suprised to hear that you are still using metal flow solder carriers.

I am based in the UK and have been using composite fixtures for many years.
We also use composite carriers for reflow soldering thin or odd shaped
PCB's.

The material that our carriers are made from is CDM (Composite Delmat
Material). This material is similar to fibre glass but a lot denser.

The material gives many benifits as listed below.

1. The Coef. of Expansion is closer to the PCB than metal is. So if the
fixture is tight damage is less likely to occur.

2. The material is a good insulator so it will not remove heat from where
you want it, namely the PCB and the solder pot.

3. Because it doesnt get so as hot, the operators manage to keep the top
layer of skin on their fingers.

4. It is very easy to modify in house.

5. The solder won't stick to it.

6. It wont bend like metal does. So it keeps the PCB's flat over the wave.

Just a few points. I'm sure that our supplier could tell you more.

Try

Von Roll Isola Ltd
TEL +44 1274 687777
FAX +44 1274 689095

This is a UK company but they may have contacts around the world.


===== Original Message from TechNet@PAT [log in to unmask] (TechNet E-Mail
Forum.) at 7/11/98 17:31
>In a message dated 11/07/98 10:58:18 AM Pacific Standard Time,
>[log in to unmask] writes:
>
>> Ironically, I had engineers from Insulfab in-house last week.  I'm
>>  evaluating composite solder pallets as an alternative to our current
>>  anodized aluminum pallets.  The technical support from a materials and
>>  mechanical engineering standpoint is very good.  The prices are also very
>>  competitive.
>>
>Doug,
>
>If you wouldn't mind, would you share what you learned about this material?
>What characteristics does this material have that make it superior to other
>types that are used for wave solder fixtures?
>
>Also, when you say the price is competitive, what would be a ballpark price
>for a fixture? I pay anywhere from $100-200 for a G10 fixture depending on
>the
>machining required...how does that compare?
>
>Thanks in Advance!
>
>-Steve Gregory-
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################


Mark Austin (Process Engineer)
ACW Technology Limited
Hylton Road
Petersfield
GU32 3XX
ENGLAND

TEL - +44 (0) 1730 300000
FAX - +44 (0) 1730 266045

Email - [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2