Doug,

Pretty cheap shot there. What are you trying to say, that I and my company
promote waste of our natural resources. If I were you I would not make any
claims that I cannot support with facts.

I would also like to challenge your statement of your reflow using one half
to one third of the N2 that our reflow systems (or any others for that
matter) use. I am sure that the people on this forum would like to see who
has the lowest N2 consumption. In addition you should mention how wide, long
and tall your process cavity is as that makes a big difference. At ETS we
compare N2 consumption to throughput.

Brian

>Hello again Brian,
>
>In my immediate defense I have to say that not only do we discourage the
>wanton waste of natural and national resources by using too much Nitrogen
>but also we offer a Reflow System that uses one-half to one-third of the
>consumption rate of any oven I have seen on the market.  Ok, ok, I'll stop
>with the tongue-in-cheek adverts =-)
>
>On to the technical issues, I would say that the effect will not be quite a
>linear relationship but it should be pretty close.  At the same flow rate
>and all variables being constant (bar the additional oxygen molecules) I
>would not see you having any problem getting under 50 ppm with a 25 - 30
>ppm source - if that is indeed what they are able to get (I suggest making
>sure they are correct about their numbers).  So, unless someone disagrees,
>I do not think the expansion rate differentail between N2 and O2 will be
>significant.  If you find out otherwise please let me know.  I may not be
>telling you anything new, but there's my two-cents.  Take care.
>
>Doug Bennett
>Sales Engineer
>Heraeus Amersil, Inc
>Atlanta, Georgia, USA
>770-623-5630 ext 4225
>
>
>
>At 03:39 PM 4/29/98 -0700, you wrote:
>>Doug,
>>
>>I appreciate your input but it does not really answer my question. I am
>>aware that by putting high amounts of N2 in the machine the customer can
>>reach the same PPM level as the source Nitrogen but no customer in their
>>right mind is going to want to pay for that. You may ask your customers to
>>do that but we look for affordable N2 processing methods for our customers.
>>Sorry, had to put at least one plug for my company just to return the favor!
>>;-)
>>
>>The real question is at the same flow rates how will the purity levels in
>>the process cavity be affected if the source is 25 - 30 ppm. Keep in mind
>>that ETS ovens run at approx 9 ppm throughout the process cavity when the
>>source is less than 5 ppm (approximately 2-3 ppm). Should the customer be
>>able to acheive less than 50 ppm (in other words add the inpurities in the
>>source to the PPM levels acheived in ETS Factory or does the expansion rate
>>of O2 affect this number)?
>>
>>I appreciate any advise offered.
>>
>>Brian
>>
>>
>>
>>
>>>Hi Brian,
>>>
>>>To answer your question they will be able to reach whatever
>>>purity level their gas is spec'ed at as long as they are willing to pay for
>>>it in total nitrogen consumption.
>>>
>>>Simply put, the spec residual oxygen level will be dependent on the
>>>internal (relative) positive pressure of the gas inside the process
>>>chamber.  Specific formulas for consumption depend on oven design so it is
>>>best to use empirical data - i.e. run experiments.  But if they crank up
>>>the internal pressure they will be able to reach those levels but they will
>>>have to pay for it, and prices of Nitrogen in Asia are quite expensive.
>>>
>>>On another note, your customer will also have fluctuating levels of
>>>residual oxygen along the length (and width for that matter) of the process
>>>chamber.  This situation depends on your configuration for feeding nitrogen
>>>into the process chamber.  So, if your customer has concerns about
>>>reliability of a steady residual oxygen level throughout the entire process
>>>chamber this could be a problem.
>>>
>>>Hope this helps
>>>
>>>Doug Bennett
>>>Sales Engineer
>>>Heraeus Amersil, Inc.
>>>Atlanta, Georgia
>>>770-623-5630 ext 4225
>>>
>>>
>>>At 04:48 PM 4/27/98 -0700, you wrote:
>>>>Dear Technet,
>>>>
>>>>My company builds reflow ovens that are capable of processing in a Nitrogen
>>>>(N2) atmosphere. We are getting ready to send an N2 machine to a
>customer in
>>>>Asia. While preparing for the installation our customer found that his
>>>>source N2 has 25 - 30 PPM of Oxygen (O2). At our factory we have source N2
>>>>that is 99.999% pure or has 1-3 PPM of O2. With this source purity level we
>>>>are able to acheive less than 20 PPM of O2 in the process cavity. With this
>>>>in mind what purity level should our Asian customer be able to acheive with
>>>>his source of 25 - 30 PPM?
>>>>
>>>>Is there a relationship between source N2 and process cavity purity levels
>>>>at constant flow rates? Does it have something to do with the expansion
>>>>rates of these gases during heating?
>>>>
>>>>Thanks in advance for all replies.
>>>>
>>>>Brian Stumm
>>>>
>>>>################################################################
>>>>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>>>>################################################################
>>>>To subscribe/unsubscribe, send a message to [log in to unmask] with
>>>following text in the body:
>>>>To subscribe:   SUBSCRIBE TechNet <your full name>
>>>>To unsubscribe:   SIGNOFF TechNet
>>>>################################################################
>>>>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>>>information.
>>>>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>>>847-509-9700 ext.311
>>>>################################################################
>>>>
>>>>
>>>
>>>
>>
>>################################################################
>>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>>################################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with
>following text in the body:
>>To subscribe:   SUBSCRIBE TechNet <your full name>
>>To unsubscribe:   SIGNOFF TechNet
>>################################################################
>>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>information.
>>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>>################################################################
>>
>>
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2