In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (105 lines)
There is no single date you can apply. If you want to do this you will have
to slog each one. Pb-free has been coming for years and already arrived in
Japan some years ago. So different suppliers will be in different stages.
Also some will have been Pb free for some time but not necessarily RoHS
compliant. Others will have been Pb-free (in the sense of not happening to
use lead finish) but not Pb-free temperature processable and so on. In
addition it is possible that any surplus non ROHS compliant stock will end
up in USA as it will not be saleable in Europe. Lets hope that you don't end
up with wooden leads from a soldering point of view....

Pragmatically
Apart from BGA Pb-free finishes are compatible with Sn63. I don't think you
will have issues soldering RoHS compliant parts with Sn63 solder. Many parts
have always used finishes which didn't happen to contain lead.
Tin whiskering is still a concern in a Pb free environment so precautions
are taken against that in RoHS compliant parts just as before. The
precautions have to be RoHS compliant so for example BI may be doped into
finish instead of Pb. This does represent a change although it may have no
functional or processing significance.




Regards

Mike Fenner
Indium Corporation

T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - Bogert
Sent: Thursday, March 23, 2006 6:46 AM
To: [log in to unmask]
Subject: [TN] Seeking date that part manufacturers started eliminating lead
from part finishes

March 23, 2006

Folks, my understanding is that about 50% of the electronic part
manufacturers have been eliminating Pb from their part finishes without also
changing their part numbers.  I am concerned that because of this, we may
inadvertently be getting lead-free parts and mixing these with lead-bearing
parts.  Concerns are possible tin-whiskers (since pure tin is sometimes used
in lieu of Pb for finishes) and solder joint issues when soldering lead-free
using Sn63 solder.

We have a lot of delivered equipment that I am trying to determine if we
could have these issues.  One way to bound the problem would be to determine
a date by when most part manufacturers starting phasing out Pb from their
part finishes.  Knowing this date, we may be able to accept equipment
manufactured prior to this date with minimum risk.  One possible date may be
the date RoHS started.

Do you folks know of a date that would give me a warm fuzzy that equipment
delivered prior to this date should not be subject to the
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
lead-free issues?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2