TECHNET Archives

December 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Linda.Li" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Linda.Li
Date:
Mon, 5 Dec 2005 16:51:09 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (89 lines)
Hello Rudy,


Thanks for your reply.


My supplier uses LPI solder mask, the dry film lamination after solder mask printing is to cover those copper patterns that are be finally coated by electrolytic plated nickel and gold,  so that they won't be contaminated during electroless nickel and immersion gold plating.



Linda Li



-----Original Message-----
From: R Sedlak [mailto:[log in to unmask]]
Sent: Friday, December 02, 2005 8:21 PM
To: TechNet E-Mail Forum; Li, Linda
Subject: Re: [TN] How to prevent solder mask peeling problem for ENIG+ENEG circuit boards



Linda Li:


I take it you are using dryfilm soldermask?   A LONG time ago, Hewlett Packard made their own PCB's, and had exactly the sort of problems you describe, and they took drastic action to resolve the matter.   At this time, the "alternate oxides" currently in use today were not heard of, and the old style alkaline black/brown oxides were in use.   We discovered that when this type of oxide was sprayed, (rather than the conventional dip tank) the oxide coating was lightened dramatically, and in fact, with some adjustment of time and temperature, we were able to give them an oxide which was invisible...BUT, it made the soldermask stick so powerfully, that the board had to be destroyed to remove the mask.  Everybody, including ourselves, was amazed at this result.  They continued using the process until they closed the shop.


I may even have some brochures around descri! bing the process.


Rudy Sedlak
RD Chemical Company

"Linda.Li" <[log in to unmask]> wrote:

Hello all,

We have a design using ENIG plus ENEG surface finishing on circuit boards, ENIG is used for Al wire bonding, ENEG is used for Au wire bonding. We met 2 problems about this design.

1) We found solder mask peeling problem after aging the assembled circuit boards at 150 degree C for 2 hours. We contact the circuit board supplier and were told that because of 2 times UV exposure( 1 time is in solder mask exposure, the other is in ENIG process), the solder mask was apt to peel off. So far the supplier doesn't have any good method to solve this problem. Do you have any suggestions to solve this problem? Thanks.
2) During ENIG process, the gold is seeped onto the surface of copper pad that needs t! o be electrolytic gold plated. It's because of air bubble entrapped during dry film lamination. The supplier has changed the lamination speed, processed the panels in different direction, but still can't solve the problem. I am in urgent need of your expert advice .

The circuit board fabrication process flow is as follows: >> solder mask printing>>dry film lamination>> UV exposure>>dry film development>>Electroless Nickel Immersion gold plating>>strip dry film resist>>Electrolytic nickel and gold plating>>

Thanks for your help in advance!

Best regards,

Linda Li




****************************************************************************************

Note: If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of thi! s communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you.

****************************************************************************************

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at sasako@i! pc.org or 847-615-7100 ext.2815
-----------------------------------------------------





  _____ 


Yahoo! Personals
Skip the bars and set-ups and start  <http://us.rd.yahoo.com/evt=36107/*http://personals.yahoo.com/us/reg/free7days> using Yahoo! Personals for free



****************************************************************************************

Note:  If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you.


***************************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
*************

ATOM RSS1 RSS2