TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Campbell, William (wcampbel)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 2 Mar 2001 14:16:47 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (63 lines)
Hi Earl-

No experience with them, but there are some new dispensers out that are
capable of placing a dot on top of a dot, "shooting" it into position- the
mfg name escapes me.

In theory, this should take up less room under the part, but still doesn't
address the root of the problem- reflowing paste and curing glue at the same
time- the respective needs are too different and leads to the glue/paste
problems we all know and love.

If you could combine the new dispenser with a glue that cures at a temp
closer to reflow, bingo.  Screen printing paste should work well too, but
can be a pain if you don't have a spare printer sitting around.

Here's hoping & good luck-

Bill C

-----Original Message-----
From: Earl Moon [mailto:[log in to unmask]]
Sent: Thursday, March 01, 2001 6:25 PM
To: [log in to unmask]
Subject: Re: [TN] RFU2


Steve.

I'll try anything and have done most but I still keep seeing epoxy in solder
joints because of tight spacing and lack of registration. How small a glue
dot can be printed/dispensed and registered without encroaching on SMT
pad/solder joint, etc.? I still have x-section nightmares bouncing around.


Thanks,

Earl

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2